PLA
FDMEasy choice for visual prototypes. Heat-sensitive.
By quoteProcess and material are separate choices. FDM fleet: Bambu Lab H2C, H2D and H2S. Pricing for each part is set in the quote.
Filament. Suited to functional parts, enclosures, jigs and fixtures, and mechanical prototypes. Layer lines are visible — that is the process. Multi-material (Dual Print) and CoreXY for short lead times.
Photopolymer resin. Suited to fine detail, tight fits and small parts. Not every resin is meant for long-term mechanical use.
Five printers from the leading series. Official H2-series motion accuracy:
0.05 mm per Bambu Lab, with the Vision Encoder. This is motion-system accuracy, not a guaranteed tolerance for every part. Dimensional accuracy depends on material and geometry — we detail it in the quote. SLA is a separate route.
Price per material: by quote. Pricing depends on the part, quantity and material, and appears in the written quote.
Easy choice for visual prototypes. Heat-sensitive.
By quoteMore heat-resistant than PLA. Good for enclosures.
By quoteLike ABS, but UV- and sun-resistant. For outdoor parts.
By quotePA filament — not powder-bed SLS.
By quoteEveryday filament for general-purpose parts.
By quoteAs easy as PETG, stiffer, matte finish.
By quotePolycarbonate. Heat and impact.
By quoteCarbon-fiber PLA. Stiff, more brittle.
By quoteGlass-fiber nylon.
By quoteFlexible. Seals and shock absorbers.
By quoteWater-soluble support. Not for end-use parts.
By quoteCarbon-fiber reinforced nylon. Mechanical stability and high temperature resistance.
By quoteResin. The resin type is specified in the written quote.
By quoteUV, chemical and heat columns come right after the material name. On narrow screens, scroll sideways.
| Material | UV resistance | Chemicals | Part heat resistance (°C) | In short | Tensile strength (MPa) | Stiffness / modulus (GPa) | Impact strength (kJ/m²) |
|---|---|---|---|---|---|---|---|
| PLA | Weak | Acetone destroys it. Water and alcohol weaken it. | 50–60 | Easy to print, almost no shrinkage. Good for prototypes. | 50–70 | 3.0–3.5 | 2.0–5.0 |
| PLA-CF PLA + carbon fiber | Weak | Like PLA. Not for chemicals. | 50–65 | Stiffer than PLA, more brittle under impact. Abrasive to nozzles. | 45–70 | 5.0–8.0 | 2.0–6.0 |
| PETG | Moderate | Water and weak acids OK. Not acetone. | 65–75 | Balance of strength and durability, low shrinkage. | 45–55 | 2.0–2.4 | 6.0–12.0 |
| PETG-CF | Moderate | Like PETG. Water OK, not acetone. | 70–85 | As easy as PETG, stiffer, matte finish. | 55–70 | 4.5–5.5 | 5.0–8.0 |
| ABS | Weak | Oils OK. Acetone dissolves it. | 85–100 | Impact- and heat-resistant. Needs an enclosed chamber, high shrinkage. | 35–45 | 1.8–2.2 | 15.0–30.0 |
| ASA | Good | Water, weak acids. Acetone dissolves it. | 90–100 | Like ABS, more resistant to UV and sun. For outdoor parts. Enclosed chamber. | 40–50 | 2.0–2.3 | 12.0–30.0 |
| Nylon (PA) | Weak | Good with oils and fuels. Not acids. Absorbs water. | 70–90 | Strong and tough, high impact resistance. Absorbs moisture — printed dry. | 60–80 | 1.5–2.5 | 20.0–40.0 |
| PA-CF nylon + carbon fiber | Weak–moderate | Like nylon: good with oils and fuels, not acids. | 150–190 | Nylon strength + carbon stiffness, almost no shrinkage. Abrasive — needs a hardened nozzle. | 80–120 | 6.0–8.5 | 8.0–12.0 |
| PA-GF nylon + glass fiber | Weak–moderate | Like nylon: good with oils and fuels, not acids. | 150–180 | Stiff and stable like PA-CF, slightly heavier. Abrasive to nozzles. | 70–110 | 5.0–8.0 | 8.0–15.0 |
| PC polycarbonate | Moderate | Water and weak acids OK. Not acetone. | 110–130 | Engineering material: heat and impact. Needs a heated chamber. | 55–70 | 2.0–2.4 | 20–40 |
| TPU | Weak–moderate | Good with oils and grease. Alcohols and ketones cause swelling. | 60–80 | Flexible. Seals, shock absorbers, covers. | 20–50 | 0.05–0.3 | Flexible |
| PVA | — | Dissolves in water. No chemical resistance. | — | Water-soluble support. Not for end-use parts. | — | — | — |
| Photopolymers SLA / resin | Weak | Depends on the resin. Standard resin yellows in sunlight. | 40–80 | Detail and tight fits. Resin type stated in the written quote. | 30–60 | 1.5–3.0 | 5–25 |
Typical values, not an order specification. Heat resistance is the HDT of the printed part (not the print temperature). UV and chemical ratings are rules of thumb for a porous FDM part, not a lab certificate. Acetone attacks ABS/ASA. PVA dissolves in water. The written quote specifies the exact material. Pricing by quote.
Pricing comes in a written quote, after we have checked the geometry.
FDM (Bambu Lab H2C, H2D, H2S) and SLA. The materials listed above are our standard range.
Metal printing is not part of the service. The farm specializes in FDM engineering plastics and SLA resins.